Effect of Hydrothermal Aging and Beverages on Color Stability of Lithium Disilicate and Zirconia Based Ceramics

التفاصيل البيبلوغرافية
العنوان: Effect of Hydrothermal Aging and Beverages on Color Stability of Lithium Disilicate and Zirconia Based Ceramics
المؤلفون: Satheesh B. Haralur, Noura Raqe S. Alqahtani, Fatimah Alhassan Mujayri
المصدر: Medicina, Vol 55, Iss 11, p 749 (2019)
بيانات النشر: MDPI AG, 2019.
سنة النشر: 2019
المجموعة: LCC:Medicine (General)
مصطلحات موضوعية: lithium disilicate, monolithic zirconia, colour stability, discolouring agents, all ceramic prosthesis, Medicine (General), R5-920
الوصف: Background and Objectives: All-ceramic prosthesis is widely used in modern dental practice because of its improved physico-mechanical and optical properties. These restorations are exposed to coloring agents from various nutrition and beverages in the oral cavity. Long-term color stability is critical for the success of these restorative materials. The purpose of this in vitro study was to assess the effect of common beverages and mouthwash on the color stability of lithium disilicate (LD), monolithic zirconia (MZ) and bilayer zirconia (BZ) surfaces. Materials and Method: Thirty disc-shaped specimens from each material were fabricated; each group was subdivided (n = 10) according to coffee, green tea and chlorhexidine immersion solutions. The baseline color of ceramic discs was recorded according to the CIE L*a*b* system with a portable spectrophotometer. The second measurement was recorded after 3000 thermocycling and immersion in coloring agents for 7 days. The mean color difference was calculated and data were compared with Kruskal-Wallis and Mann-Whitney post hoc tests (0.05). Results: ΔE values for LD with the immersion of coffee, tea, and Chlorhexidine gluconate (CHG) were 1.78, 2.241 and 1.58, respectively. Corresponding ΔE values for MZ were 5.60, 5.19, and 4.86; marginally higher than the clinically acceptable level of 3.5. Meanwhile, BZ showed better color stability compared to MZ with ΔE values of 4.22, 2.11 and 1.43. Conclusions: Among the ceramics evaluated, LD ceramic was found to be more color stable, while MZ ceramics displayed a higher susceptibility to discoloration. MZ and BZ ceramic colors were significantly altered with coffee immersion, while LD ceramics were more affected by green tea.
نوع الوثيقة: article
وصف الملف: electronic resource
اللغة: English
تدمد: 1010-660X
Relation: https://www.mdpi.com/1010-660X/55/11/749; https://doaj.org/toc/1010-660X
DOI: 10.3390/medicina55110749
URL الوصول: https://doaj.org/article/64ce48025bd0495ab96c142991015a07
رقم الانضمام: edsdoj.64ce48025bd0495ab96c142991015a07
قاعدة البيانات: Directory of Open Access Journals
الوصف
تدمد:1010660X
DOI:10.3390/medicina55110749