Academic Journal

An experimental investigation on the influence of volume fraction using Straw fiber on the bending and tensile strength of material composites

التفاصيل البيبلوغرافية
العنوان: An experimental investigation on the influence of volume fraction using Straw fiber on the bending and tensile strength of material composites
المؤلفون: Arifin, Agus Choirul, Majedi, Farid, Bisono, Rahayu Mekar, Fakhrudi, Yoga Ahdiat, Al. Aziz.R, M. Shafwallah
المصدر: International Journal of Science, Engineering and Information Technology; Vol 8, No 1 (2023): IJSEIT Volume 08 Issue 01 31 December 2023; 437-441 ; International Journal of Science, Engineering, and Information Technology; Vol 8, No 1 (2023): IJSEIT Volume 08 Issue 01 31 December 2023; 437-441 ; 2548-4214 ; 10.21107/ijseit.v8i1
بيانات النشر: Universitas Trunojoyo Madura
سنة النشر: 2023
المجموعة: Jurnal Universitas Trunojoyo Madura
مصطلحات موضوعية: Rice straw fiber, composite, natural fibers, bending and tensile strength, hand lay up, filler, matrix
الوصف: Rice straw fiber is considered as agricultural residue that has not been widely used other than as animal feed. In addition, the development of composite material technology that uses natural fibers provides interesting mechanical properties to be developed. This paper aims to investigate the effect of different concentrations of fiber usage on bending and tensile strength. The comparison of concentrations of fiber usage are 35% , 40% , 70% dan 80%. The straw fiber was decreased the moisture content using a microwave and the treatment with NaOH for removed the hemicellulose and lignin in the fibers. The manufacture of this biocomposite uses a matrix of Urea Formaldehyde with a hand lay up technique. The results of the mechanics test(bending and tensile strengths) show that the strength value obtained on the straw fiber variation, namely the highest average value of the Tensile test is 4.82 MPa at a ratio of 40 : 60, while the lowest is 2.88 MPa at a comparison 35 : 65 and and the highest average value of the bending test is at a ratio of 80:20 (6.64 N/mm2), while the lowest is 40:60 (2.45 N/mm2).
نوع الوثيقة: article in journal/newspaper
وصف الملف: application/pdf
اللغة: English
Relation: https://journal.trunojoyo.ac.id/ijseit/article/view/22612/pdf; https://journal.trunojoyo.ac.id/ijseit/article/view/22612
DOI: 10.21107/ijseit.v8i1.22612
الاتاحة: https://journal.trunojoyo.ac.id/ijseit/article/view/22612
https://doi.org/10.21107/ijseit.v8i1.22612
Rights: Copyright (c) 2023 Agus Choirul Arifin, Farid Majedi, Rahayu Mekar Bisono, Yoga Ahdiat Fakhrudi, M. Shafwallah Al. Aziz.R ; https://creativecommons.org/licenses/by-sa/4.0
رقم الانضمام: edsbas.1BE313D2
قاعدة البيانات: BASE
الوصف
DOI:10.21107/ijseit.v8i1.22612