Development and application of HVOF sprayed spinel protective coating for SOFC interconnects
العنوان: | Development and application of HVOF sprayed spinel protective coating for SOFC interconnects |
---|---|
المؤلفون: | Maija Mäkinen, Olivier Thomann, Tomi Suhonen, Markus Rautanen, Jari Kiviaho, Mikko Pihlatie, Olli Himanen, Juha Lagerbom, Tommi Varis |
المصدر: | Thomann, O, Pihlatie, M, Rautanen, M, Himanen, O, Lagerbom, J, Mäkinen, M, Varis, T, Suhonen, T & Kiviaho, J 2013, ' Development and application of HVOF sprayed spinel protective coating for SOFC interconnects ', Journal of Thermal Spray Technology, vol. 22, no. 5, pp. 631-639 . https://doi.org/10.1007/s11666-012-9880-9 |
بيانات النشر: | Springer, 2013. |
سنة النشر: | 2013 |
مصطلحات موضوعية: | Materials science, spinel, Scanning electron microscope, chemistry.chemical_element, engineering.material, law.invention, stack testing, Chromium, Coating, ASR, law, Materials Chemistry, SOFC, Thermal spraying, ProperTune, protective coating, interconnect, Metallurgy, Spinel, Condensed Matter Physics, Evaporation (deposition), Cathode, Surfaces, Coatings and Films, chemistry, HVOF spraying, engineering, Solid oxide fuel cell |
الوصف: | Protective coatings are needed for metallic interconnects used in solid oxide fuel cell (SOFC) stacks to prevent excessive high-temperature oxidation and evaporation of chromium species. These phenomena affect the lifetime of the stacks by increasing the area-specific resistance (ASR) and poisoning of the cathode. Protective MnCo2O4 and MnCo1.8Fe0.2O4 coatings were applied on ferritic steel interconnect material (Crofer 22 APU) by high velocity oxy fuel spraying. The substrate-coating systems were tested in long-term exposure tests to investigate their high-temperature oxidation behavior. Additionally, the ASRs were measured at 700 °C for 1000 h. Finally, a real coated interconnect was used in a SOFC single-cell stack for 6000 h. Post-mortem analysis was carried out with scanning electron microscopy. The deposited coatings reduced significantly the oxidation of the metal, exhibited low and stable ASR and reduced effectively the migration of chromium. |
اللغة: | English |
تدمد: | 1544-1016 1059-9630 |
DOI: | 10.1007/s11666-012-9880-9 |
URL الوصول: | https://explore.openaire.eu/search/publication?articleId=doi_dedup___::cc1c9bffb8839dc552779247afabe977 https://cris.vtt.fi/en/publications/bb929f97-5f5b-4e4c-967d-f59991212a3e |
Rights: | CLOSED |
رقم الانضمام: | edsair.doi.dedup.....cc1c9bffb8839dc552779247afabe977 |
قاعدة البيانات: | OpenAIRE |
تدمد: | 15441016 10599630 |
---|---|
DOI: | 10.1007/s11666-012-9880-9 |