Crystal Orientation Modulation and Defect Passivation for Efficient and Stable Methylammonium-Free Dion-Jacobson Quasi-2D Perovskite Solar Cells

التفاصيل البيبلوغرافية
العنوان: Crystal Orientation Modulation and Defect Passivation for Efficient and Stable Methylammonium-Free Dion-Jacobson Quasi-2D Perovskite Solar Cells
المؤلفون: Shi Chen, Jiangzhao Chen, Le Bai, Hua Yang, Xiaobing Cao, Dongmei He, Zhigang Zang, Huan Bi, Donghwa Lee, Pengyu Su, Baibai Liu, Wenqi Wang
المصدر: ACS Applied Materials & Interfaces. 13:29567-29575
بيانات النشر: American Chemical Society (ACS), 2021.
سنة النشر: 2021
مصطلحات موضوعية: Materials science, Passivation, Energy conversion efficiency, 02 engineering and technology, 010402 general chemistry, 021001 nanoscience & nanotechnology, 01 natural sciences, Grain size, 0104 chemical sciences, Crystallinity, Formamidinium, Chemical engineering, Phase (matter), Molecule, General Materials Science, 0210 nano-technology, Perovskite (structure)
الوصف: Dion-Jacobson (DJ) quasi-2D perovskite solar cells (PSCs) have received increasing attention due to their greater potentials in realizing efficient and stable quasi-2D PSCs relative to their Ruddlesden-Popper counterpart. The substitution of methylammonium (MA+) with formamidinium is expected to be able to further increase the stability and power conversion efficiency (PCE) of DJ quasi-2D PSCs. Herein, we report a multifunctional additive strategy for preparing high-quality MA-free DJ quasi-2D perovskite films, where 1,1'-carbonyldi(1,2,4-triazole) (CDTA) molecules are incorporated into the perovskite precursor solution. CDTA modification can control phase distribution, enlarge grain size, modulate crystallinity and crystal orientation, and passivate defects. After CDTA modification, more favorable gradient phase distribution and accordingly gradient band alignment are formed, which is conducive to carrier transport and extraction. The improved crystal orientation can facilitate carrier transport and collection. The enlarged grain size and effective defect passivation contribute to reduced defect density. As a result, the CDTA-modified device delivers a PCE of 16.07%, which is one of the highest PCEs ever reported for MA-free DJ quasi-2D PSCs. The unencapsulated device with CDTA maintains 92% of its initial PCE after aging under one sun illumination for 360 h and 86% after aging at 60 °C for 360 h.
تدمد: 1944-8252
1944-8244
DOI: 10.1021/acsami.1c05498
URL الوصول: https://explore.openaire.eu/search/publication?articleId=doi_dedup___::b523d408b65cff51eae200f202108a45
https://doi.org/10.1021/acsami.1c05498
Rights: CLOSED
رقم الانضمام: edsair.doi.dedup.....b523d408b65cff51eae200f202108a45