Academic Journal

Development of stabilization measures aimed at removing zinc with smelting products and accumulating titanium in the hearth of a blast furnace.

التفاصيل البيبلوغرافية
العنوان: Development of stabilization measures aimed at removing zinc with smelting products and accumulating titanium in the hearth of a blast furnace.
المؤلفون: Semenov, Yurii, Horupakha, Viktor, Vashchenko, Serhii, Khudyakov, Oleksandr, Shumelchyk, Ievhen, Baiul, Kostiantyn
المصدر: Engineering Reports; Oct2024, Vol. 6 Issue 10, p1-13, 13p
مصطلحات موضوعية: BLAST furnaces, ZINC smelting, PULVERIZED coal, THERMAL coal, CAST-iron, SMELTING furnaces
مستخلص: This paper presents the results of the development of stabilization measures aimed at the removal of zinc with the products of melting and accumulation of titanium in the hearth of a blast furnace. The relevance of the development and use in practice of such measures is due to the unstable fuel and raw materials conditions for the production of cast iron, when their stabilization is a complex and difficult task, as well as the need to extend the campaign of blast furnaces during the overhaul period. The negative effect of zinc oxides on the condition of the blast furnace shaft lining, accompanied by slab formation, and the overconsumption of specific coke consumption, which occurs when zinc circulates in the volume of the blast furnace, require measures to remove zinc from the smelting products. The article proposes such measures, which consist of flushing according to the proposed schedule during the operation of the blast furnace at planned blowing parameters and with the provision of the necessary thermal reserve. In order to lengthen the campaign of a blast furnace, one of the most common methods for protecting the hearth lining is the periodic introduction of titanium‐containing materials into the charge of blast furnaces. The entry of titanium oxides into the furnace, as a rule, is ensured by the use of concentrate or specially prepared ilmenite briquettes with a high titanium content as part of the sinter charge, which can be introduced directly into the composition of the blast furnace charge. The article analyzes the experience of using titanium‐containing materials as part of a blast furnace charge and formulates measures to intensify skull formation in the hearth. [ABSTRACT FROM AUTHOR]
Copyright of Engineering Reports is the property of Wiley-Blackwell and its content may not be copied or emailed to multiple sites or posted to a listserv without the copyright holder's express written permission. However, users may print, download, or email articles for individual use. This abstract may be abridged. No warranty is given about the accuracy of the copy. Users should refer to the original published version of the material for the full abstract. (Copyright applies to all Abstracts.)
قاعدة البيانات: Complementary Index
الوصف
تدمد:25778196
DOI:10.1002/eng2.12881